Physical Properties
Metric
English
Comments
Fiber Count
220
dtex
198
denier
GB/T14335-2008
Sichuan Deyang Haton® 220 dtex Polyphenylene Sulfide Filament
Excellent chemical stabilityInformation provided by Sichuan Deyang Chemical Co., LTD