Polymer Property : Fiber Count = 22.0 dtex Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 11.0 - 22.0 dtex
9.90 - 19.8 denier
EMS-Griltech Grilon® CM 2600 White Nylon 6 Fiber
Description: GRILON CM 2600 is a Nylon 6 technical fiber which is used to produce technical felts.Data provided by EMS-Griltech.
Fiber Count 17.0 - 22.0 dtex
15.3 - 19.8 denier
EMS-Griltech Grilon® TN 2200 White Nylon 6 Fiber
Description: GRILON TN 2200 is used for woolen yarns which is then further processed to produce technical fabrics.Applications: Press Felt FabricData provided by EMS-Griltech.