Polymer Property : Fiber Count = 3.30 dtex Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Fiber Count 3.30 - 6.70 dtex
2.97 - 6.03 denier
EMS-Griltech Grilon® BA 3100 White Nylon 66/Nylon 6 Bi-Component Fiber
Description: GRILON BA 3100 is the new core / sheath bi-component fiber based on PA 66/PA 6 with a sheath melting range from 215 - 225 °C. The fine count bi-component fiber guarantees an even distr..
Fiber Count 3.30 dtex
2.97 denier
EMS-Griltech Grilamid® HP 1200 Nylon 12 Fiber (Staple Length = 51)
Description: GRILAMID HP 1200 is a Nylon 12 fiber used in hybrid yarns and as a matrix in composite materials.Data provided by EMS-Griltech.
Fiber Count 3.30 dtex
2.97 denier
EMS-Griltech Grilon® BA 115 White Nylon 6/CoPA Bi-Component Fiber
Description: GRILON BA 115 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 110 - 120 °C. The fine count bi-component fiber guarantees an even distrib..
Fiber Count 3.30 - 4.20 dtex
2.97 - 3.78 denier
EMS-Griltech Grilon® M 369 White Nylon 6 Fiber
Description: GRILON M 369 is a fine PA6 fiber with soft interlinings for special thermobonding properties and low shrinkage in the soft end product. The coarser counts, 3.3 - 4.2 dtex, are also used..
Fiber Count 3.30 dtex
2.97 denier
EMS-Griltech Grilon® M 371 White Nylon 6 Fiber
Description: GRILON M 371 is a durable siliconized fine fiber for very soft, thermobonded interlinings. The coarser counts, 3.3 - 4.8 dtex, are also used for volume nonwovens and cotton yarns. Data ..