Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 405 dtex | 365 denier | Warp yarn; Twaron® 1055 |
Hexcel® HexForce™ 5348 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Fiber Count | 405 dtex | 365 denier | Fill yarn; Twaron® 1055 |
Hexcel® HexForce™ 5348 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Fiber Count | 405 dtex | 365 denier | Warp yarn; Twaron® 1055 |
Hexcel® HexForce™ 5351 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Fiber Count | 405 dtex | 365 denier | Fill yarn; Twaron® 1055 |
Hexcel® HexForce™ 5351 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |