Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 8.00 dtex | 7.20 denier | |
EMS-Griltech Grilon® BA 140 White Nylon 66/CoPA Bi-Component Fiber Description: GRILON BA 140 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 135 - 145 °C. The fine count bi-component fiber guarantees an even distrib.. |