Physical Properties Metric English Comments
Fiber Count 9.40 - 10.6 dtex
8.46 - 9.54 denier
Voloknohim TU 6-13-5-99 Nylon 6
Application: for textile industry and other purposes and carpet-market industry. The produced yarn is round: crimped, bright, semi dull, not dyed and dyed in mass. Information provided by Voloknokhi..