Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Permeability | 0.0900 g mil/ (m2 day) @Temperature 37.0 °C |
0.00581 g mil/ (100 in2 day) @Temperature 98.6 °F |
90% RH; ASTM E96 |
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating Parylene D is a polymer of para-xylylene modified by the substitution of chlorine atoms for two of the aromatic hydrogen atoms. Parylene D is similar in properties to Parylene C with the added abili.. |