Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | -0.000670 cm/cm | -0.000670 in/in | Cold Part VS Cold Tool, Expansion; ASTM D955 |
Applied Composites 185 Polyester SMC Industry Application: TransportationProduct Application: Lawn and GardenDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation. |