Polymer Property : Linear Mold Shrinkage = 0.0013 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0013 cm/cm
0.0013 in/in
ATM D955
Plenco 50030 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..
Linear Mold Shrinkage 0.0013 cm/cm
0.0013 in/in
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced
Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent..
Linear Mold Shrinkage 0.0013 cm/cm
0.0013 in/in
ASTM D955
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Linear Mold Shrinkage 0.0013 - 0.0035 cm/cm
0.0013 - 0.0035 in/in
Bulk Molding Compounds BMC 6605A Polyester Molding Compound