Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00183 cm/cm
0.00183 in/in
ASTM D955
Plenco 05118-T5 Phenolic, Granular, Compression Molded
PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve..