Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | |
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ATM D955 |
Plenco 50045 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ISO 2577 |
Polyram RamSter PF300G8 PBT, 40% Glass Fiber 40% Glass fiber reinforced PBT for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | 320 x 320 mm flat plaque; ISO 1183 |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ASTM D2566-69 |
BCC Products BC 7062-3H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ASTM D955 |
Techmer Lehvoss Compounds Luvotech™ J-4/30 BK PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ASTM D955 |
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 BK2989 PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ASTM D955 |
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 NAT PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ASTM D955 |
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 RD6922 PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ASTM D955 |
Techmer Lehvoss Compounds Luvotech™ J-4/35 BK223 PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ASTM D955 |
Techmer Lehvoss Compounds Luvotech™ J-4/35 NAT PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Linear Mold Shrinkage | 0.0027 cm/cm | 0.0027 in/in | ASTM D955 |
Techmer Lehvoss Compounds Luvotech™ J-4/35/HS NAT PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |