Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00298 cm/cm | 0.00298 in/in | ASTM D955 |
Plenco 3509 Phenolic, Granular, Transfer Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |