Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0020 - 0.0038 cm/cm
0.0020 - 0.0038 in/in
Bulk Molding Compounds BMC T9 General Purpose Molding Compound
BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9..
Linear Mold Shrinkage 0.0026 - 0.0038 cm/cm
0.0026 - 0.0038 in/in
IS 13411-1992
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded
Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit..
Linear Mold Shrinkage 0.0030 - 0.0038 cm/cm
0.0030 - 0.0038 in/in
IS 13411-1992
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color..