Polymer Property : Linear Mold Shrinkage = 0.0067 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
ASTM D955-89
Multibase Multi-Pro® 2010 X Natural 20% Filler Content Polypropylene
Data provided by Multibase.
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
ASTM D955
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
ASTM D955
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
ASTM D955
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
ASTM D955
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
Plastcom SLOVAMID 6 GF 10 FRC 2 PA6, 10% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 10 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an..
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
STN 64 0808
Plastcom SLOVAMID 6 GF 15 LS Polyamide 6, 15% Glass Fiber, UV Stabilization
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools...
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
Plastcom SLOVAMID 6 GF 15 MI/2 PA6, 15% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
Kostat 7440 Conductive ABS Compound
KOSTAT 7440 is a conductive thermoplastic compound based on Acrylonitrile Butadiene Styrene and a special carbon black. KOSTAT 7440 is not dependant on atmospheric conditions and is used for ESD in..
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
ASTM D955
Plenco 4002 Phenolic, Granular, Injection Molded
PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi..
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
ASTM D955
Plenco 4309 Phenolic, Nodular, Injection Molded
PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430..