Polymer Property : Linear Mold Shrinkage = 0.0089 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0081 - 0.0089 cm/cm
0.0081 - 0.0089 in/in
IS 13411-1992
Amity Thermosets ATM 123 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownMedium flow..