Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00900 cm/cm
0.00900 in/in
ASTM D955
Niche Polymer PA66MI40BK Nylon 66, 40% Mineral Fiber Filled, Impact Modified
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00900 cm/cm
0.00900 in/in
ASTM D955
Niche Polymer PA66MI40N Nylon 66, 40% Mineral Fiber Filled, Impact Modified
Information provided by Niche Polymer