Polymer Property : Linear Mold Shrinkage = 0.0099 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0099 cm/cm
0.0099 in/in
ASTM D955
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0099 cm/cm
0.0099 in/in
STN 64 0808
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
Linear Mold Shrinkage 0.0099 cm/cm
0.0099 in/in
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Linear Mold Shrinkage 0.0099 cm/cm
0.0099 in/in
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Linear Mold Shrinkage 0.0099 cm/cm
0.0099 in/in
Isotropy
Solvay TECHNYL® C 236SI PA6, DRY
Description: Unreinforced polyamide 6 with high impact strength for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® C 236SI has high impact strength and fle..