Polymer Property : Linear Mold Shrinkage = 0.0126 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0126 cm/cm
0.0126 in/in
ASTM D955
Multibase Multi-Flex® TPE D 5302 NAT
The moisture content is 0.912%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Linear Mold Shrinkage 0.0126 cm/cm
0.0126 in/in
STN 64 0808
Plastcom SLOVAMID 6 FRC 2 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization
FeaturesLongterm external use is possible because of the material stabilization with the light stabilizers on the HALS basis. Meets the flammability in accordance with the norm DIN 4102 - B1. PA 6..
Linear Mold Shrinkage 0.0126 cm/cm
0.0126 in/in
ASTM D955
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade
Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0126 cm/cm
0.0126 in/in
ASTM D955
PolyOne Synprene® IT 454 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerApplications:General PurposeCove BaseInteriorMarket:AutomotiveConsumer GoodsBuilding and ConstructionProcessing Method:Extrusion and Molding..