Polymer Property : Linear Mold Shrinkage = 0.0129 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0129 cm/cm
0.0129 in/in
ASTM D955
Multibase Multi-Flex® TPE D 4310
Multi-Flex® D 4310 Natural was designed to replace Himont's CA 53 G material. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Linear Mold Shrinkage 0.0129 cm/cm
0.0129 in/in
Plastcom SLOVAMID 66 MI PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..