Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0136 cm/cm
0.0136 in/in
Plastcom SLOVALEN PC 51 C 20 PP, 20% mineral filling
FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C..
Linear Mold Shrinkage 0.0136 cm/cm
0.0136 in/in
STN EN ISO 294-4
Plastcom SLOVALEN PC 51 C 40 LS/1M Polypropylene reinforced with mineral filler, UV stabilized
Modified copolymer PP for injection molding with the content of 40% mineral filler, UV stabilized. Product meets glow wire test at 750°C. Delivered in full RAL color scale.Information Provided by P..
Linear Mold Shrinkage 0.0136 cm/cm
0.0136 in/in
STN 64 0808
Plastcom SLOVALEN PC 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc
FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C...
Linear Mold Shrinkage 0.0136 cm/cm
0.0136 in/in
Plastcom SLOVALEN PC 51 C 40 PP reinforced with 40% mineral filler
Features: Modified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified chalk. Increased strength, rigidity and thermal application up to 100..
Linear Mold Shrinkage 0.0136 cm/cm
0.0136 in/in
Plastcom SLOVALEN PC 91 C 20 PP, 20% mineral filling
FeaturesModified copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C depending on th..