Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0177 cm/cm | 0.0177 in/in | STN 64 0808 |
Plastcom SLOVALEN PC 52 T 20 Polypropylene Copolymer, 20% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Linear Mold Shrinkage | 0.0177 cm/cm | 0.0177 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 79 GF 20 Polypropylene Homopolymer, 20% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |