Linear Mold Shrinkage 0.0178 cm/cm
0.0178 in/in
STN 64 0808
Plastcom SLOVALEN PC 51 C 30 Polypropylene Homopolymer and Copolymer, 30% Micronized Talc
FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 30% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C...