Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0195 cm/cm | 0.0195 in/in | |
Plastcom SLOVALEN PC 51 GF 10 PP, 10% glass fibre FeaturesModified copolymer PP for injection moulding, chemically reinforced with 10% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suitabl.. |
|||
Linear Mold Shrinkage | 0.0195 cm/cm | 0.0195 in/in | |
Plastcom SLOVALEN PC 81 T 15 PP, 15% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 15% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Linear Mold Shrinkage | 0.0195 cm/cm | 0.0195 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 41 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit.. |