Linear Mold Shrinkage 0.0202 cm/cm
0.0202 in/in
Plastcom SLOVALEN PQ 81 T 25 PP, 25% mineral filling
FeaturesModified PP for injection moulding with the content of 25% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shri nkage. Gen..