Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00800 - 0.0226 cm/cm | 0.00800 - 0.0226 in/in | Average value: 0.0143 cm/cm Grade Count:26 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0226 cm/cm | 0.00100 - 0.0226 in/in | Average value: 0.00526 cm/cm Grade Count:33 |