Polymer Property : Linear Mold Shrinkage = 0.0238 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0238 cm/cm
0.0238 in/in
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant
FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin..