Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0256 cm/cm
0.0256 in/in
STN EN ISO 294-4
Plastcom PLASTAMID® 6 HI PA6 with improved impact strength
PA 6 for injection molding, impacted, modified with thermoplastic elastomer, determined for high impacted moldings also at low temperature. Delivered in natural mode and in the full RAL color scale...
Linear Mold Shrinkage 0.0256 cm/cm
0.0256 in/in
Plastcom SLOVAMID 6 LI PA6, improved strength
FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme..