Polymer Property : Linear Mold Shrinkage = 0.0386 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00240 - 0.0386 cm/cm
0.00240 - 0.0386 in/in
Average value: 0.0145 cm/cm Grade Count:7
Overview of materials for Polycarbonate-Urethane
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr..