Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00100 - 0.0550 cm/cm | 0.00100 - 0.0550 in/in | Average value: 0.00760 cm/cm Grade Count:191 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Linear Mold Shrinkage | 0.000400 - 0.0550 cm/cm | 0.000400 - 0.0550 in/in | Average value: 0.00459 cm/cm Grade Count:661 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |