Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.787 g/cc @Temperature 25.0 °C |
0.787 g/cc @Temperature 77.0 °F |
|
Indium Corp. 16-1085 Flux Thinner 16-1085 flux thinner is for use with Wave Solder Flux 1085, to maintain specific gravity during use.Physical PropertiesColor: ClearInformation provided by the manufacturer, Indium Corporation of Am.. |