Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.791 g/cc @Temperature 25.0 °C |
0.791 g/cc @Temperature 77.0 °F |
|
Indium Corp. NR-10-D Wave Solder Flux, No-Clean Wave Solder Flux #NR-10-D is a low-solids, rosin/resin-free flux. It is specially formulated to be used for wave soldering where the cleaning process has been eliminated. Any post-soldering residu.. |