Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.000035 cm/cm
0.000035 in/in
Solvay TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY
Description: Polyamide 6, 30% glass fiber reinforced, for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 1021GF6 is used in all sectors of industry, offering an excelle..