Polymer Property : Linear Mold Shrinkage, Flow = 0.00050 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00010 - 0.00050 cm/cm

@Time 86400 sec
0.00010 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP ECL36XXQ PEI
LNP* Lubricomp* ECL36XXQ is a compound based on Polyetherimide containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.00010 - 0.00050 cm/cm

@Time 86400 sec
0.00010 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP EC008 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EC008 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00010 - 0.00050 cm/cm

@Time 86400 sec
0.00010 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI
LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow.
Linear Mold Shrinkage, Flow 0.00010 - 0.00050 cm/cm

@Time 86400 sec
0.00010 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI
LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing
Linear Mold Shrinkage, Flow 0.00030 - 0.00050 cm/cm

@Time 86400 sec
0.00030 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DC0049XF PC
LNP* THERMOCOMP* DC0049XF is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.