Polymer Property : Linear Mold Shrinkage, Flow = 0.00199 in/in
Polymer Property :
Linear Mold Shrinkage, Flow =
0.00199 in/in
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Linear Mold Shrinkage, Flow
0.00199
cm/cm
0.00199
in/in
ISO 294-4, 2577
Lanxess Pocan® B 2505 000000 PBT
PBT, non-reinforced, injection molding, flame retardant