Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0020 - 0.0023 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0023 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP 30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0023 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0023 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Asia Pacific) 30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |