Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Thickness 2.00 mm
0.0028 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
Zytel® BM73G15THS is a 15% glass fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Temperature 80.0 °C
0.0028 in/in

@Temperature 176 °F
60x60x2 mm; ISO 294-4
Gromax BFG30-FU00B3 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Linear Mold Shrinkage, Flow 0.0028 cm/cm
0.0028 in/in
ISO 294-4, 2577
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
Linear Mold Shrinkage, Flow 0.0028 cm/cm
0.0028 in/in
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Thickness 3.20 mm
0.0028 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin.
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Thickness 3.20 mm
0.0028 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® IQNH4560 PBT (Asia Pacific)
Valox* IQNH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin.
Linear Mold Shrinkage, Flow 0.0028 cm/cm
0.0028 in/in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* WF006 is a compound based on Polybutylene Terephalate resin containing Glass Fiber.
Linear Mold Shrinkage, Flow 0.0028 cm/cm
0.0028 in/in
ISO Data
BASF Ultradur B 4406 G6 Q113 30% Glass Filled PBT
Ultradur B4406 G6 Q113 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement.
Linear Mold Shrinkage, Flow 0.0028 cm/cm
0.0028 in/in
ISO 294
BASF Ultrason E 2010 G6 30% Glass Filled PES
Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.