Linear Mold Shrinkage, Flow 0.00200 - 0.00300 cm/cm
0.00200 - 0.00300 in/in
Compression; ISO 2577
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..