Linear Mold Shrinkage, Flow 0.0047 cm/cm
0.0047 in/in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific)
LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0047 cm/cm

@Time 86400 sec
0.0047 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific)
LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated.