Polymer Property : Linear Mold Shrinkage, Flow = 0.00600 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00200 - 0.00600 cm/cm
0.00200 - 0.00600 in/in
Injection; ISO 2577
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
Linear Mold Shrinkage, Flow 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
Compression; ISO 2577
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Linear Mold Shrinkage, Flow 0.00400 - 0.00600 cm/cm
0.00400 - 0.00600 in/in
Injection and Compression; ISO 2577
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
Linear Mold Shrinkage, Flow 0.00500 - 0.00600 cm/cm
0.00500 - 0.00600 in/in
Compression; ISO 2577
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..