Linear Mold Shrinkage, Flow 0.0067 cm/cm
0.0067 in/in
ISO 294-4
DSM EcoPaXX® Q-PG6 PA410-I-GF30
% Glass Reinforced, Impact Modified
Linear Mold Shrinkage, Flow 0.0067 cm/cm
0.0067 in/in
ISO 294-4
DSM EcoPaXX® Q-X07208 PA410-I-GF30
% Glass Reinforced, Impact Modified