Linear Mold Shrinkage, Flow
0.005
-
0.008
cm/cm
0.005
-
0.008
in/in
ASTM D955
Clariant Renol PA143G10 Nylon 6/66 Copolymer, 10% Glass Fiber, Heat Stabilized
Data provided by Clariant Masterbatches