Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0084 cm/cm
0.0084 in/in
ISO 294-4
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY
Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go..