Polymer Property : Linear Mold Shrinkage, Flow = 0.0127 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0127 cm/cm
0.0127 in/in
Solvay TECHNYL® A 221 Natural FA PA66, DRY
Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv..