Polymer Property : Linear Mold Shrinkage, Flow = 0.0225 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0225 cm/cm
0.0225 in/in
Annealed; ISO 294-4
DuPont Performance Polymers Crastin® S600F40 NC010 PBT  (Unverified Data**)
Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.0225 - 0.0265 cm/cm
0.0225 - 0.0265 in/in
LATI Latan 23UVE71 POM
Polyoxymethylene (POM). UV stabilized. Toughened. Low viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..