Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 25.4 cm | 10.0 in | Melt temperature at 330°C; Spiral mold 1.5 x 6 mm; 17 mm for 10MFR PC resins |
LG Chemical Lupoy 3010-15 Polycarbonate Resin Description: LUPOY PC 3010-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Spiral Flow | 25.4 cm | 10.0 in | Melt temperature at 330°C; Spiral mold 1.5 x 6 mm; 17 mm for 10MFR PC resins |
LG Chemical Lupoy 3030-15 Polycarbonate Resin Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |