Polymer Property : Spiral Flow = 12.0 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 12.0 cm

@Thickness 1.00 mm
4.72 in

@Thickness 0.0394 in
370°C nozzle, 170°C tool
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..