Polymer Property : Spiral Flow = 16.7 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 42.4 cm
16.7 in
Equistar test
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Spiral Flow 42.5 cm
16.7 in
240°C; DENKA method
Denka STYROL MW1 Polystyrene
"DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," ..