Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 53.3 - 119 cm
21.0 - 47.0 in
Average value: 79.0 cm Grade Count:62
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..