Physical Properties Metric English Comments
Spiral Flow 25.0 - 76.0 cm
9.84 - 29.9 in
Average value: 58.5 cm Grade Count:13
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..