Physical Properties Metric English Comments
Spiral Flow 95.0 cm
37.4 in
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i..
Spiral Flow 95.0 - 117 cm
37.4 - 46.1 in
Average value: 99.2 cm Grade Count:9
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Spiral Flow 95.0 cm

@Thickness 2.00 mm,
Temperature 250 °C
37.4 in

@Thickness 0.0787 in,
Temperature 482 °F
Borealis Method
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced
Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st..
Spiral Flow 95.0 cm
37.4 in
Cross Section: 7[mm]x3.5[mm]; AKRO
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Spiral Flow 95.0 cm
37.4 in
Cross Section: 7[mm]x3.5[mm]; AKRO
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..